  • Article
    Citation - WoS: 44
    Citation - Scopus: 54
    Protection of Marble Surfaces by Using Biodegradable Polymers as Coating Agent
    (Elsevier, 2009) Ocak, Yılmaz; Sofuoğlu, Aysun; Tıhmınlıoğlu, Funda; Böke, Hasan
    Biodegradable polymers have been replaced over the synthetic polymers in many applications due to their good properties such as reversibility and biodegradability. Therefore they allow new treatment on the surface of the material to be protected and they fulfil the principles generally accepted by the International Conservation Community of Historic Monuments and Buildings. In this study, the efficiency of four different biodegradable polymers as protective coatings on marble-SO2 reaction was investigated. The polymers used were zein, chitosan, polyhydroxybutyrate (PHB), and poly-l-lactide (PLA). The mineralogical composition, bulk density and porosity of uncoated marble were determined. The water vapor permeability, water absorption by capillary forces, surface wettability, and color alteration of uncoated and coated marbles were measured. For sulphation reaction, marble slabs were coated with these polymers and then they were exposed at nearly 8 ppm SO2 concentration at 100% relative humidity conditions together with uncoated ones in a reaction chamber for several days for testing their protection efficiency. The extent of reaction was determined by leaching of gypsum formed on the marble surfaces in deionized water and then determining the sulphate content by ion chromatography. The protection efficiency of polymer treatments was expressed as comparing the gypsum crust thickness of the coated and uncoated marble plates. The comparison among the polymers showed that the surface hydrophobicity, water capillary absorption and structure of polymer would be important factors affecting the protection efficiency. The use of high molecular weight PLA (HMWPLA) polymer on marble surfaces provided significant protection up to 60% which was indicated that HMWPLA polymer seems to be promising polymer as protective coating agent in reducing gypsum formation on marble surfaces in the polluted environment.
  • Article
    Citation - WoS: 8
    Citation - Scopus: 8
    Reducing Marble-So2 Reaction Rate by the Application of Certain Surfactants
    (Springer Verlag, 2003) Böke, Hasan; Gauri, K. Lal
    Sulfur dioxide (SO2), prevalent in the modern urban environment of industrial countries, attacks calcite (CaCO3) in marble. As a result, a gypsum (CaSO4.2H2O) crust is produced at rain-sheltered surfaces while areas exposed to rain experience accelerated erosion. We have investigated the effect of certain surfactants as protective agents against SO2 attack. We report that the anions oxalate (C2O4-2) and oleate (C17H33COO-) from solutions of their highly soluble alkali salt species are able to replace carbonate (CO3-2) in calcite producing less reactive substrate of oxalate and oleate of calcium. Experiments to measure the protection obtained by these treatments were carried out in the laboratory and field conditions at nearly 1 ppm and 10 ppb SO2 concentrations, respectively. We found that these treatments provided significant protection to marble exposed in sheltered areas, up to 30% reduction of reaction rate by treatment with 2 × 10-4 M sodium oleate and up to 14% by a 2 × 10-3 M with potassium oxalate solutions, but become ineffective over long term exposure when applied to surfaces exposed to rain. Carrara marble was used in the reported study. Ion chromatography was the analytical tool, which allowed precise measurements of ionic concentrations of these salts, the amount of their uptake by marble, and the thickness of the gypsum crust. X-ray diffraction allowed determination of the new minerals formed at the marble surface by the treatment with surfactants.