    Investigation of the High Temperature Dry Sliding Wear Behavior of Graphene Nanoplatelets Reinforced Aluminum Matrix Composites
    (SAGE Publications, 2021) Martin, Seçkin; Kandemir, Sinan; Antonov, M.
    In this study, graphene nanoplatelets (GNPs) with a thickness of 50-100 nm have been utilized to improve the mechanical and tribological properties of A360 alloy due to their extraordinary mechanical properties and solid lubricant nature. For the investigation of tribological properties, ball-on disc tests were carried out at various temperatures including room temperature (RT), 150 °C, and 300 °C. According to the hardness and ball-on-disc test results, the nanocomposite samples reinforced with GNPs exhibited improved hardness and wear resistance. The improvement in the wear behavior of nanocomposites was referred to the temporarily formed solid lubricant film of harder GNPs during the wear, and hence coefficient of friction (COF) and volume loss were considerably reduced. Abrasive-adhesive, oxidative, and mild-to-severe were found to be main wear mechanisms at RT, 150 °C, and 300 °C, respectively. Overall, the results show that the nanocomposites fabricated by casting method combined with mechanical stirring and ultrasonication have promising wear performance, especially at elevated temperatures. This may suggest that these developed materials could be potential candidates to be used in the engineering applications requiring high temperature wear performance. © The Author(s) 2020.
  • Article
    Citation - WoS: 4
    Citation - Scopus: 5
    Effects of Tib2 Nanoparticle Content on the Microstructure and Mechanical Properties of Aluminum Matrix Nanocomposites
    (Walter de Gruyter GmbH, 2017) Kandemir, Sinan
    The present work reports the fabrication of A357 alloy matrix nanocomposites reinforced with 0.5, 1.0 and 2.0 wt.-% TiB2 nanoparticles (20-30 nm) by a novel method which is the combination of semi-solid mechanical mixing and ultrasonic dispersion of nanoparticles in liquid state. The microstructural and mechanical properties of the fabricated nanocomposites were investigated. The microstructural studies conducted with optical and advanced electron microscopes indicated that reasonably effective deagglomeration and uniform distribution of TiB2 nanoparticles into the matrix were achieved. Transmission electron microscopy studies also confirmed that the nanoparticles were embedded into the matrix and a good bonding was obtained between the matrix and the reinforcement. Increasing nanoparticle content led to grain refinement and significant enhancement in the mechanical properties of nanocomposites. The addition of 0.5, 1.0, and 2.0 wt.-% TiB2 nanoparticles increased the 0.2 % proof stress of matrix alloy by approximately 31, 48 and 61 %, respectively. The contribution of different mechanisms to the strength enhancement is discussed. It is proposed that the strengthening is mainly due to Orowan mechanism and dislocation generation effect by the coefficient of thermal expansion mismatch between the TiB2 nanoparticles and the matrix.
  • Conference Object
    Development of Graphene Nanoplatelets Reinforced Aluminium Matrix Nanocomposites by a Combination of Semi-Solid Stirring and Ultrasonic Treatment
    (European Conference on Composite Materials, 2016) Kandemir, Sinan; Aydoğan, Yücel
    Graphene Nanoplatelets (GNPs) consisting of graphene layers with a thickness less than 100 nm have recently emerged as a promising reinforcement type owing to their excellent physical and mechanical properties to improve mechanical properties of alloys beyond ceramic nanoparticles. Although there are numerous studies on GNPs reinforced polymer matrix composites in the literature, the number of studies related to the incorporation of GNPs in metal matrices is limited. It is a challenging task to incorporate and uniformly distribute GNPs into liquid metals due to their poor wettability and large surface-to-volume ratio. The purpose of this study is to effectively disperse GNPs into liquid aluminium. 0.5 wt.% GNPs with an average thickness of 50-100 nm and size of 5 ?m were first incorporated into A360 aluminium alloy under semi-solid stirring, and then the composite was ultrasonically treated in fully liquid state. The microstructural investigation of the nanocomposites by optical and scanning electron microscopy may suggest that relatively uniform distribution and effective deagglomeration of GNPs in the matrix were achieved. The hardness of the GNPs reinforced nanocomposites increased in comparison with that of semi-solid stirred and ultrasonically processed A360 alloy without reinforcement, indicating the potential of GNPs for strengthening metals. © 2016, European Conference on Composite Materials, ECCM. All rights reserved.
  • Article
    Citation - WoS: 14
    Citation - Scopus: 16
    Microstructure and Mechanical Properties of A357/Sic Nanocomposites Fabricated by Ultrasonic Cavitation-Based Dispersion of Ball-Milled Nanoparticles
    (SAGE Publications Inc., 2017) Kandemir, Sinan
    In this work, A357/0.5 wt.% SiC nanocomposites were fabricated with a combination of ultrasonic processing and a nanoparticle feeding mechanism that involves the introduction of a closed end aluminium tube filled with the ball-milled SiC nanoparticles (20-30 nm) and aluminium powders (<75 μm) into the melt for complete deagglomeration and uniform dispersion of nanoparticles through the matrix. The microstructural and mechanical properties of the fabricated nanocomposites were investigated. The microstructural studies conducted with optical and advanced electron microscopes indicate that relatively effective deagglomeration and uniform dispersion of SiC nanoparticles into the molten alloy were achieved. The hardness and tensile properties of the nanocomposites were notably improved compared to those of the ultrasonically processed A357 alloy without reinforcement, showing the strengthening potency of nanoparticles and the good bonding obtained at the particle-reinforcement interface.