    Fructose Dehydration To 5-Hydroxymethylfurfural Over Sulfated Tio2-Sio2, Ti-Sba Zro2, Sio2, and Activated Carbon Catalysts
    (American Chemical Society, 2015) Kılınç, Emre; Yılmaz, Selahattin; Yılmaz, Selahattin; 03.02. Department of Chemical Engineering; 03. Faculty of Engineering; 01. Izmir Institute of Technology
    Different sulfated catalysts including SO4/TiO2-SiO2, SO4/Ti-SBA-15, SO4/ZrO2, SO4/AC, and SO4/SiO2 were tested in fructose dehydration to 5-hydroxymethylfurfural (HMF). Reactions were carried out in dimethyl sulfoxide (DMSO) at 110 °C. Characterization results indicated that no sulfur leaching was observed from SO4/ZrO2, SO4/TiO2-SiO2, and SO4/Ti-SBA-15 catalysts in the reaction tests. The SO4/TiO2-SiO2 catalyst had a high amount of strong acid sites and the highest amount of Bronsted sites. The highest selectivity to HMF at high conversion, that is, 89% selectivity at 77% fructose conversion was obtained over this catalyst. It preserved its activity after four times reuse.Activated carbonCarbonCatalystsDehydration
  • Article
    Citation - WoS: 23
    Citation - Scopus: 28
    Direct Liquefaction of High-Sulfur Coals: Effect of the Catalyst, the Solvent, and the Mineral Matter
    (American Chemical Society, 2002) Gözmen, Belgin; Artok, Levent; Erbatur, Gaye; Erbatur, Oktay; 04.01. Department of Chemistry; 04. Faculty of Science; 01. Izmir Institute of Technology
    Two low-rank coals with high sulfur contents (Gediz subbituminous coal: 7.6 wt % S:dry basis. Çayirhan lignite: 5.7 wt% S:dry basis.) were subjected to hydroliquefaction. Liquefaction conditions included dry or solvent mediated runs under pressurized hydrogen without added catalyst or with the impregnated catalyst precursor ammonium heptamolybdate (AHM). Gediz coal having higher sulfur content gave 90% conversion in the absence of catalyst and solvent. Maximum conversion (98%) and maximum oil + gas yield (70%) from this coal were obtained by impregnating AHM onto coal and carrying out liquefaction in H 2/tetralin system at 450 °C for 30 min. Under the same conditions, Çayirhan lignite gave 85% conversion and 70.5% oil + gas yield. The superior hydrodesulfurization effect of impregnated AHM on the oil fraction when used in the absence of solvent (less than 0.1% S in lignite's oil and less than 1% S in subbituminous coal's oil following one-stage hydrogenation) is a promising finding of this work. AHM was found to be much more effective in liquefaction of Çayirhan lignite and this has been ascribed to the well-dispersion of AHM throughout this lignite's structure via a cation-exchange mechanism through oxygen functionalities. Strong evidence for the catalytic effect of clay minerals in coal structure on char-forming reactions during liquefaction was observed by making use of liquefaction reactions of demineralized coal samples. It was also observed that tetralin had a retarding effect on the condensation and subsequent cross-linking reactions.