    Boosting Up Printability of Biomacromolecule Based Bio-Ink by Modulation of Hydrogen Bonding Pairs
    (Elsevier Ltd., 2020) Köksal, Büşra; Önbaş, Rabia; Başkurt, Mehmet; Şahin, Hasan; Arslan Yıldız, Ahu; Yıldız, Ümit Hakan
    This study describes low dose UV curable and bioprintable new bioink made of hydrogen bond donor-acceptor adaptor molecule 2-isocyanatoethyl methacrylate (NCO)modified gelatin (NCO-Gel). Our theoretical calculations demonstrate that insertion of 2-isocyanatoethyl methacrylate doubles the interaction energy (500 meV) between gelatin chains providing significant contribution in interchain condensation and self-organization as compared to methacrylic anhydride modified gelatin (GelMA). The NCO-Gel exhibits peak around 1720 cm?1 referring to bidentate hydrogen bonding between H-NCO and its counterpart O[dbnd]CN[sbnd]H. These strong interchain interactions drive chains to be packed and thereby facilitating UV crosslinking. The NCO-Gel is exhibiting a rapid, 10 s gelation process by the exposure of laser (3 W, 365 nm). The dynamic light scattering characterization also reveals that NCO-Gel has faster sol to gel transition as compared to GelMA depending on the UV curing time. The NCO-Gel was found to be more firm and mechanically strong that provides advantages in molding as well as bioprinting processes. Bioprinted NCO-Gel has shown sharp borders and stable 3D geometry as compared to GelMA ink under 10 s UV curing time. The cell viability tests confirm that NCO-Gel facilitates cell proliferation and supports cell viability. We foresee that NCO-Gel bioink formulation provides a promising opportunity when low dose UV curing and rapid printing are required. © 2020 Elsevier Ltd
  • Article
    Citation - WoS: 24
    Citation - Scopus: 26
    Self-Assembly Behavior of the Keratose Proteins Extracted From Oxidized Ovis Aries Wool Fibers
    (Elsevier Ltd., 2019) Pakkaner, Efecan; Yalçın, Damla; Uysal, Berk; Top, Ayben
    Water soluble keratose proteins were obtained from an Ovis Aries wool using peracetic acid oxidation. The wool samples and the extracted keratose proteins were characterized by using FTIR, XRD, SEM and TGA techniques. Fractions of alpha-keratose (MW = 43-53 kDa) along with protein species with molecular weights between 23 kDa and 33 kDa were identified in the SDS-PAGE analysis result of the extracted protein mixture. DLS and AFM experiments indicated that self-assembled globular nanoparticles with diameters between 15 nm and 100 nm formed at 5 mg/ml keratose concentration. On the other hand, upon incubation of 10 w % keratose solutions at 37 degrees C and 50 degrees C, interconnected keratose hydrogels with respective storage modulus (G') values of 0.17 +/- 0.03 kPa and 3.7 +/- 0.5 kPa were obtained. It was shown that the keratose hydrogel prepared at 37 degrees C supported L929 mouse fibroblast cell proliferation which suggested that these keratose hydrogels could be promising candidates in soft tissue engineering applications. (C) 2018 Elsevier B.V. All rights reserved.
  • Article
    Citation - WoS: 17
    Citation - Scopus: 20
    Preparation and Characterization of Antibacterial Cobalt-Exchanged Natural Zeolite/Poly(vinyl Alcohol) Hydrogels
    (Springer Verlag, 2014) Narin, Güler; Bulut Albayrak, Çisem; Ülkü, Semra
    In the present study, potential application of the local clinoptilolite-rich natural zeolite in formulation of antibacterial hydrogels was investigated. The zeolite powder exchanged with cobalt(II) ions was used in preparation of the zeolite/poly(vinyl alcohol) hydrogel films in different amounts. The films were physically crosslinked by the freezing-thawing method and characterized for their crystallinity, surface and cross sectional morphology, chemical composition, thermal behaviour, mechanical properties, swelling and dissolution behaviours, and antibacterial activities against a Gram-negative bacteria. The films with 0.48 wt% and higher cobalt-exchanged zeolite contents showed antibacterial activity. Addition of the zeolite powder in the formulations did not cause significant changes in the other properties of the films.