Scopus İndeksli Yayınlar Koleksiyonu / Scopus Indexed Publications Collection
Permanent URI for this collectionhttps://hdl.handle.net/11147/7148
Browse
4 results
Search Results
Now showing 1 - 4 of 4
Book Part Citation - Scopus: 2Influence of Filler Surface Modification on the Properties of Pp Composites(Wiley, 2015) Balköse, DevrimThis chapter reviews the fillers have been grouped as silica, glass, silicates, magnesium hydroxide and eggshell, cellulose and carbon, and their surface modification techniques. It explains the effects of the surface modification of fillers on the properties of composite materials having polypropylene as the matrix. The surface modification of fillers affects the properties of the polypropylene matrix composites in different aspects depending on the types of the filler and the modifications. The polypropylene phase was also functionalized by treating PP with MA or ammines. The properties most affected are the tensile strength, Young modulus, and elongation at break of the composites. If crosslinking occurs between the filler and functionalized PP, the tensile strength increases and elongation at break decreases owing to decrease in mobility. PP crystallite formation at the interface also increases the adhesion between filler and matrix. © 2015 Wiley-VCH Verlag GmbH & Co. KGaA. All rights reserved.Article Citation - WoS: 40Citation - Scopus: 45Comparison of Liquid Hot Water, Very Dilute Acid and Alkali Treatments for Enhancing Enzymatic Digestibility of Hazelnut Tree Pruning Residues(Elsevier, 2018) Sabancı, Kevser; Büyükkileci, Ali OğuzThe effect of pretreatments on the composition of the hazelnut tree pruning residue (HTPR) and on the digestibility of the cellulose was investigated. The liquid hot water (LHW) and the very dilute acid (VDA) treatments were effective in solubilizing hemicellulose. The cellulose conversion increased up to around 60% (corresponding to 32–36 g/L glucose) with decreasing hemicellulose concentration in the pretreated HTPR. The alkali treatment provided partial delignification, however, the glucose production was comparably lower. Combining the hemicellulose removal and the delignification effect of different pretreatments in two-stage processes (LHW-alkali and VDA-alkali treatments) enhanced the cellulose concentration in the solids, but not the amount of glucose released in the enzymatic digestion. These results suggested that the hemicellulose was the main barrier against the conversion of cellulose in the LHW and VDA treated HTPR and the glucose in the hydrolysis medium inhibited the cellulase activity, which prevented the complete conversion of cellulose.Article Citation - WoS: 9Citation - Scopus: 10Novel Hybrid Process for the Conversion of Microcrystalline Cellulose To Value-Added Chemicals: Part 2: Effect of Constant Voltage on Product Selectivity(Springer Verlag, 2017) Akın, Okan; Yüksel, AslıIn this study, electrochemical degradation of microcrystalline cellulose (MCC) under hot-compressed water was investigated via application of constant voltage on reaction medium. Constant voltage ranges from 2.5 to 8.0 V was applied between anode (Titanium) and cathode (reactor wall). As an electrolyte and proton source 5–25 mM of H2SO4 was used. Reactions were carried out in a specially designed batch reactor (450 mL) made of T316 for 240 min at temperature of 200 °C.MCC decomposition products such as glucose, fructose, furfural, 5-HMF and levulinic acid were detected and quantified by High Performance Liquid Chromatography (HPLC). In the absence of electrolyte, applied voltage (2.5 and 4.0 V) decreased the total organic carbon (TOC) yield, in contrast at 8.0 V, TOC yield increased to 13%. Application of 8.0 V in hydrothermal conditions alter MCC decomposition pathway selectively to furfural (15%). Addition of electrolyte (5 mM, H2SO4) and application of 2.5 V potential increased TOC (54%) and changed the decomposition pathway in favor of 5-HMF (30%) and levulinic acid (21%). The structural changes in solid residues of electrochemically reacted MCC was analyzed by Fourier Transform Infrared Spectroscopy (FTIR) and found that MCC particles functionalized by carboxylic acid and sulfonated groups by the application of constant voltage to reaction medium. In the presence of electrolyte, under certain voltage (2.5 V), functionalization of solid particles became more obvious in FTIR spectrum results. Therefore, change in the selectivity values of degradation products were conducted with the functionalization of MCC particles due to applied voltage under sub-critical conditions.Article Citation - WoS: 11Citation - Scopus: 12Novel Hybrid Process for the Conversion of Microcrystalline Cellulose To Value-Added Chemicals: Part 1: Process Optimization(Springer Verlag, 2016) Akın, Okan; Yüksel, AslıIn this paper, a novel hybrid process for the treatment of microcrystalline cellulose (MCC) under hot-compressed water was investigated by applying constant direct current on the reaction medium. Constant current range from 1A to 2A was applied through a cylindrical anode made of titanium to the reactor wall. Reactions were conducted using a specially designed batch reactor (450 mL) made of SUS 316 stainless steel for 30–120 min of reaction time at temperature range of 170–230 °C. As a proton donor H2SO4 was used at concentrations of 1–50 mM. Main hydrolysis products of MCC degradation in HCW were detected as glucose, fructose, levulinic acid, 5-HMF, and furfural. For the quantification of these products, High Performance Liquid Chromatography (HPLC) and Gas Chromatography with Mass Spectroscopy (GC–MS) were used. A ½ fractional factorial design with 2-level of four factors; reaction time, temperature, H2SO4 concentration and applied current with 3 center points were built and responses were statistically analyzed. Response surface methodology was used for process optimization and it was found that introduction of 1A current at 200 °C to the reaction medium increased Total Organic Carbon (TOC) and cellulose conversions to 62 and 81 %, respectively. Moreover, application of current diminished the necessary reaction temperature and time to obtain high TOC and cellulose conversion values and hence decreased the energy required for cellulose hydrolysis to value added chemicals. Applied current had diverse effect on levulinic acid concentration (29.9 %) in the liquid product (230 °C, 120 min., 2 A, 50 mM H2SO4). © 2016, Springer Science+Business Media Dordrecht.