Scopus İndeksli Yayınlar Koleksiyonu / Scopus Indexed Publications Collection
Permanent URI for this collectionhttps://hdl.handle.net/11147/7148
Browse
4 results
Search Results
Now showing 1 - 4 of 4
Article Citation - WoS: 23Citation - Scopus: 31Nano-Caco3 Synthesis by Jet Flow(Elsevier Ltd., 2017) Ülkeryıldız, Eda; Kılıç, Sevgi; Özdemir, EkremA new methodology was introduced to produce hollow nano calcite particles in homogenous size distribution without aggregation. The design consisted of a jet flow system in which the crystallization region was separated from the stabilization region. The newly produced nano CaCO3 particles of about 140 nm were removed from the crystallization region as quickly as possible into the stabilization region before aggregation or crystal growth. In the stages of crystallization, the particles started to dissolve from their edges which opened-up the pores inside the particles. At the late stages of crystallization, the open pores closed. These particles were stable in Ca(OH)2 solution and no aggregation was detected. Different particles with different morphologies can be produced by adjusting the stages in the crystallization.Article Citation - WoS: 20Citation - Scopus: 23Rice-Like Hollow Nano-Caco3 Synthesis(Elsevier Ltd., 2016) Ülkeryıldız, Eda; Kılıç, Sevgi; Özdemir, EkremWe have shown that Ca(OH)2 solution is a natural stabilizer for CaCO3 particles. We designed a CO2 bubbling crystallization reactor to produce nano-CaCO3 particles in homogenous size distribution without aggregation. In the experimental set-up, the crystallization region was separated from the stabilization region. The produced nanoparticles were removed from the crystallization region into the stabilization region before aggregation or crystal growth. It was shown that rice-like hollow nano-CaCO3 particles in about 250 nm in size were produced with almost monodispersed size distribution. The particles started to dissolve through their edges as CO2 bubbles were injected, which opened-up the pores inside the particles. At the late stages of crystallization, the open pores were closed as a result of dissolution-recrystallization of the newly synthesized CaCO3 particles. These particles were stable in Ca(OH)2 solution and no aggregation was detected. The present methodology can be used in drug encapsulation into inorganic CaCO3 particles for cancer treatment with some modifications.Article Citation - WoS: 12Citation - Scopus: 13Statistical Thermal Stability of Pvc(John Wiley and Sons Inc., 2010) Atakul Savrık, Sevdiye; Cansever Erdoğan, Beyhan; Balköse, Devrim; Ülkü, SemraExperimental design was used to optimize the processing parameters for the decomposition of poly (vinyl chloride). Factorial design and face centered composite design (FCC) were applied to determine the optimum conditions. A total of 10 g PVC powder was mixed with different amounts of zinc stearate (ZnSt 2) and natural zeolite and tested for thermal stability. Factorial fitted model was explained by first order pattern due to the significant main effect regression constants, and FCC model was described by second order model owing to higher order polynomial coefficients. FCC design was superior to factorial design as FCC considers not only its pure quadratic effects contribution but also its higher overall desirability for thermal stability of PVC. For factorial design the optimum conditions were determined as 163.06 mg for ZnSt2, 399.99 mg for zeolite, and 140°C for temperature with desirability of 0.933. However, 400 mg for ZnSt2, 333.24 mg for zeolite, and 140°C for temperature with desirability of 0.956 were obtained as the optimum conditions by FCC design. © 2010 Wiley Periodicals, Inc.Article Citation - WoS: 8Citation - Scopus: 5Tin Soaps in Emulsion Pvc Heat Stabilization(John Wiley and Sons Inc., 2002) Arkış, Esen; Balköse, DevrimIn this study, the effect of a liquid stabilizer based on organotins on PVC heat stability is investigated. Control and films with tin soap heat stabilizer Sn500K were prepared by solvent casting and they were heated at 160 and 180°C for different time periods. X-ray fluorescence spectroscopy analysis showed that tin was present in Sn500K and it was lead-free. DSC analysis showed that glass-transition temperature of films with Sn500K increased from 67 to 75-85°C by heating for 15 min at 180°C. IR spectroscopy indicated that concentration of carboxylate groups of Sn500K decreased with heating. Films with Sn500K did not degrade for short heating periods; however, degradation occurred in long heating times. Low concentration of Sn500K was recommended, since at high levels incompatibility with PVC and acceleration of degradation was observed. In the high temperature range, control and stabilized samples degraded in the same manner in two steps