WoS İndeksli Yayınlar Koleksiyonu / WoS Indexed Publications Collection

Permanent URI for this collectionhttps://hdl.handle.net/11147/7150

Browse

Search Results

Now showing 1 - 2 of 2
  • Article
    Citation - WoS: 66
    Citation - Scopus: 79
    Piping Network Design of Geothermal District Heating Systems: Case Study for a University Campus
    (Elsevier Ltd., 2010) Yıldırım, Nurdan; Toksoy, Macit; Gökçen, Gülden
    Geothermal district heating system design consists of two parts: heating system and piping network design. District heating system design and a case study for a university campus is given in Yildirim et al. [1] in detail. In this study, piping network design optimisation is evaluated based on heat centre location depending upon the cost and common design parameters of piping networks which are pipe materials, target pressure loss (TPL) per unit length of pipes and installation type. Then a case study for the same campus is presented. © 2010 Elsevier Ltd.
  • Article
    Testing Corrosion Rates on Steel Piping in Geothermal District Heating
    (National Association of Corrosion Engineers, 2008) İnce, Umut; Toksoy, Macit; Güden, Mustafa
    The corrosion behavior of St-37 pipeline carbon steel (CS) in a geothermal district heating system was tested at two different fluid velocities. An experimental set-up, directly connected the the end of the transmission line of a geothermal well, was used to assess the corrosion of St-37 steel tensile test coupons prepared in accordance with ASTM E8 in geothermal fluid. The geothermal fluid entered the set-up with a relatively low velocity, 0.02 m/s, and then injected into the well with a relatively high fluid velocity, 9.6 m/s. It was observed that while the uniform corrosion rates were relatively low, pitting corrosion rate, mainly driven by the sulfate-reducing bacteria (SRB) activity, was relatively high and more pronounced at low fluid velocities. St-37 steel material is prone to the pitting type corrosion, thus a biocide chemical addition and the fluid velocity of 2 to 3 m/s in transmission line were recommended to reduce SRB activity to reduce the pitting corrosion rate.