    Statistical Thermal Stability of Pvc
    (John Wiley and Sons Inc., 2010) Atakul Savrık, Sevdiye; Cansever Erdoğan, Beyhan; Balköse, Devrim; Ülkü, Semra
    Experimental design was used to optimize the processing parameters for the decomposition of poly (vinyl chloride). Factorial design and face centered composite design (FCC) were applied to determine the optimum conditions. A total of 10 g PVC powder was mixed with different amounts of zinc stearate (ZnSt 2) and natural zeolite and tested for thermal stability. Factorial fitted model was explained by first order pattern due to the significant main effect regression constants, and FCC model was described by second order model owing to higher order polynomial coefficients. FCC design was superior to factorial design as FCC considers not only its pure quadratic effects contribution but also its higher overall desirability for thermal stability of PVC. For factorial design the optimum conditions were determined as 163.06 mg for ZnSt2, 399.99 mg for zeolite, and 140°C for temperature with desirability of 0.933. However, 400 mg for ZnSt2, 333.24 mg for zeolite, and 140°C for temperature with desirability of 0.956 were obtained as the optimum conditions by FCC design. © 2010 Wiley Periodicals, Inc.
  • Article
    Citation - WoS: 18
    Citation - Scopus: 19
    Effect of Zeolite Filler on the Thermal Degradation Kinetics of Polypropylene
    (John Wiley and Sons Inc., 2006) Pehlivan, Hilal; Balköse, Devrim; Ülkü, Semra; Tıhmınlıoğlu, Funda
    In this study, the thermal degradation behavior of polypropylene (PP) and PP-zeolite composites was investigated, Clinoptilolite, a natural zeolitic tuff, was used as the filler material in composites. The effects of both pure clinoptilolite and silver-ion-exchanged clinoptilolite on the thermal degradation kinetics of the PP composites was studied with differential scanning calorimetry (DSC) and thermogravimetric analysis (TGA). Polymer degradation was evaluated with DSC at heating rates of 5, 10, and 20°C/ min from room temperature to 500°C. The silver concentration (4.36, 27.85, and 183.8 mg of Ag/g of zeolite) was the selected parameter under consideration. From the DSC curves, we observed that the heat of degradation values of the composites containing 2-6% silver-exchanged zeolite (321-390 kj/kg) were larger than that of the pure PP (258 kj/kg). From the DSC results, we confirmed that the PPzeolite composites can be used at higher temperatures than the pure PP polymer because of its higher thermal stability, The thermal decomposition activation energies of the composites were calculated with both the Kissinger and Ozawa models. The values predicted from these two equations were in close agreement. From the TGA curves, we found that zeolite addition into the PP matrix slowed the decomposition reaction; however, silver-exchanged zeolite addition into the matrix accelerated the reaction. The higher the silver concentration was, the lower were the thermal decomposition activation energies we obtained. As a result, PP was much more susceptible to thermal decomposition in the presence of silver-exchanged zeolite.