  • Article
    Citation - WoS: 8
    Citation - Scopus: 10
    Experimental and Computational Investigation of Graphene/Sams Schottky Diodes
    (Elsevier Ltd., 2018) Aydın, Hasan; Bacaksız, Cihan; Senger, Ramazan Tuğrul; Karakaya, Caner; Mermer, Ömer; Selamet, Yusuf; Senger, Ramazan Tuğrul; Şahin, Hasan; Şahin, Hasan; 04.04. Department of Photonics; 04.05. Department of Pyhsics; 04. Faculty of Science; 01. Izmir Institute of Technology
    We have investigated the effect of two different self-assembled monolayers (SAMs) on electrical characteristics of bilayer graphene (BLG)/n-Si Schottky diodes. Novel 4″bis(diphenylamino)-1, 1′:3″-terphenyl-5′ carboxylic acids (TPA) and 4,4-di-9H-carbazol-9-yl-1,1′:3′1′-terphenyl-5′ carboxylic acid (CAR) aromatic SAMs have been used to modify n-Si surfaces. Cyclic voltammetry (CV) and Kelvin probe force microscopy (KPFM) results have been evaluated to verify the modification of n-Si surface. The current–voltage (I–V) characteristics of bare and SAMs modified devices show rectification behaviour verifying a Schottky junction at the interface. The ideality factors (n) from ln(I)–V dependences were determined as 2.13, 1.96 and 2.07 for BLG/n-Si, BLG/TPA/n-Si and BLG/CAR/n-Si Schottky diodes, respectively. In addition, Schottky barrier height (SBH) and series resistance (R s ) of SAMs modified diodes were decreased compared to bare diode due to the formation of a compatible interface between graphene and Si as well as π–π interaction between aromatic SAMs and graphene. The CAR-based device exhibits better diode characteristic compared to the TPA-based device. Computational simulations show that the BLG/CAR system exhibits smaller energy-level-differences than the BLG/TPA, which supports the experimental findings of a lower Schottky barrier and series resistance in BLG/CAR diode.
  • Article
    Citation - WoS: 21
    Citation - Scopus: 27
    Increasing Solubility of Metal Silicates by Mixed Polymeric Antiscalants
    (Elsevier Ltd., 2019) Topçu, Gökhan; Çelik, Aslı; Demir, Mustafa Muammer; Baba, Alper; Şahin, Hasan; Çelik, Aslı; Baba, Alper; Şahin, Hasan; 03.09. Department of Materials Science and Engineering; 04.04. Department of Photonics; 03.03. Department of Civil Engineering; 03. Faculty of Engineering; 04. Faculty of Science; 01. Izmir Institute of Technology
    The increase of silicate solubility is a big challenge for both hot and cold water because it reduces the deposition of metal silicates frequently observed in such systems and causes operational obstacles. The deposition of silicate coats the inner surface of the pipelines in an uncontrolled manner and reduces the harvesting of energy from brines. In this work, the solubility performance of two commercial water-soluble polymeric agents (poly(ethylene glycol) (PEG) and poly(vinyl alcohol) (PVA)) of various molecular weights employing dosage from 25 to 100 mg/L was examined. Along with dispersant-type antiscalant, poly(acrylamide) (PAM), poly(vinylsulfonic acid, sodium salt) (PVSA), and poly(vinylphosphonic acid) (PVPA) having chelating acidic groups were employed. Metal silicate deposits were obtained artificially in the lab-scale pressurized reactor. The experimental conditions employed were quite similar to a model power plant located in Çanakkale, Turkey. The concentration of dissolved silica was increased from 130 to 420 mg/L when 100 mg/L PEG 1500 and 25 mg/L PVSA were employed as a mixture. For the atomic-level understanding of the interaction of chelating groups with metal cations, DFT calculations were performed too.