The Spheroidization Behavior of Low Alloy White Cast Iron and Its Effect on Impact Toughness and Wear Resistance

Loading...

Date

Journal Title

Journal ISSN

Volume Title

Open Access Color

Green Open Access

No

OpenAIRE Downloads

OpenAIRE Views

Publicly Funded

No
Impulse
Average
Influence
Average
Popularity
Average

relationships.isProjectOf

relationships.isJournalIssueOf

Abstract

The effect of spheroidization on impact toughness and wear resistance, together with the spheroidization kinetics of a low alloy white cast iron (LAWCI) have been studied. Spheroidization process was carried out using two different routes; intercritical annealing and subcritical annealing both of which were followed by furnace cooling to room temperature. Both routes involve a process window, which is determined by holding time and temperature. For the intercritical annealing the spheroidization window is significantly shorter (0.5-3 h) than the conventional subcritical spheroidization (6 - 12 h); and that process window narrows with increasing intercritical annealing temperature. The intercritical spheroidization involves 3 distinct stages; (i) partial, followed by (ii) fully spheroidization of lamellar pearlitic matrix by divorced eutectoid transformation (DET); and (iii) partially spheroidization by pearlitic structure formation in previous fully spheroidized region. The end of third stage produces almost fully pearlitic matrix, which is coarser than the as-cast condition. In case of subcritical spheroidization, the process window opens after about 6 hours and the size of spherical carbides gets larger with time. The as-cast LAWCI having a microstructure composed of eutectic carbide network and pearlite matrix exhibits and impact toughness of 4.6 J. Spheroidization process not only changes the lamellar pearlitic structure into spheroidized carbides but also slightly reduces the amount of eutectic carbides. Those microstructural changes greatly improve the impact toughness of LAWCI up to 11.8 J; whereas some decrease in the wear resistance. For spheroidized LAWCI, mean diameter of carbides (D), interparticle spacing of carbides (s), and number of carbides per area (n) seems to be important microstructural variations to determine the impact toughness and wear properties. Taking properties of the current material into consideration, spheroidized white cast irons may be a viable alternative material for industrial applications, offering a trade-off between wear resistance and toughness.

Description

Keywords

Spheroidization, Process Window, Divorced Eutectoid Transformation (Det), White Cast Iron, Impact Toughness, Wear Performance

Fields of Science

Citation

WoS Q

Scopus Q

OpenCitations Logo
OpenCitations Citation Count
N/A

Volume

1011

Issue

Start Page

End Page

PlumX Metrics
Citations

Scopus : 2

Captures

Mendeley Readers : 2

Google Scholar Logo
Google Scholar™
OpenAlex Logo
OpenAlex FWCI
0.33868835

Sustainable Development Goals