Abstract
The aim of this study was to prepare phase pure tetracalcium phosphate (TTCP) from the precursor phase mixtures homogeneous at the nano/microscale level at lower heat treatment temperatures in much shorter dwell times. Two different precursor powder mixtures were prepared by reacting CaCO3 with H3PO4 in ethanol or water. The resultant precursor powder mixtures were heat treated at temperatures in the 1200-1350 degrees C range for 2 and 5 h. Phase structures of the powders were characterized by X-ray diffraction (XRD), Fourier transform infrared (FTIR) and Raman spectroscopy analysis. Scanning electron microscopy (SEM) was used for the investigation of powder particle sizes and morphology. Powders synthesized by the heat treatment of both of the starting powder mixtures prepared in ethanol or water with 2 and 5 h of dwell times at 1350 degrees C were determined to be phase pure TTCP. SEM analysis along with the phase identification showed that the precursor powder prepared in ethanol had micron sized plates formed by aggregation of sub-micron sized thin CaHPO4 plates covering CaCO3 particles. The precursor powder prepared in water contained large aggregates of sub-micron sized CaCO3 particles whose surface was covered by precipitated nano-sized hydroxyapatite. TTCP powders were composed of large irregularly shaped particles formed by sintering of smaller equiaxed grains. Average grain and particles sizes of the TTCP powders synthesized from the precursor powder prepared in ethanol were 3.2-3.9 and 8.1-8.4 mu m, respectively. Average grain and particle sizes of the TTCP powders synthesized from the precursor powder prepared in water however were measured to be 3.3-5.1 and 11.2-11.6 mu m, respectively. The TTCP preparation method presented in this study provides homogeneous and well-mixed precursor powders prepared from cheap and commonly available precursors without milling and decreases the heat treatment time to 2 h at 1350 degrees C.
Description
Cetin, Ali Emrah/0000-0002-1468-6221
Keywords
Tetracalcium Phosphate, Calcium Carbonate, Phosphoric Acid, Thermal Treatment
Fields of Science
Citation
WoS Q
Scopus Q

OpenCitations Citation Count
N/A
Source
Volume
51
Issue
1
Start Page
664
End Page
684
PlumX Metrics
Citations
Scopus : 0
Captures
Mendeley Readers : 2
Page Views
50
checked on Apr 28, 2026
Google Scholar™